Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 30.7 g/micron | 780 g/mil | ASTM D1922 |
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Elmendorf Tear Strength, TD | 30.7 g/micron | 780 g/mil | ASTM D1922 |
ExxonMobil LL 3201.36 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Elmendorf Tear Strength, TD | 30.7 g/micron | 780 g/mil | ASTM D1922 |
ExxonMobil LL 3201.69 Premium High Strength Film Resin Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al.. |
|||
Elmendorf Tear Strength, TD | 30.7 g/micron | 780 g/mil | ASTM D1922 |
ExxonMobil HD 7845.30 MMW Blown Film Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |