Elmendorf Tear Strength, TD 16.0 - 31.0 g/micron
406 - 787 g/mil
Average value: 20.1 g/micron Grade Count:18
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade