Polymer Property : Elmendorf Tear Strength, TD = 33.17 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 33.17 g/micron
842.5 g/mil
ASTM D1922
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de..