Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, TD = 35.8 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 35.8 g/micron
910 g/mil
ASTM D1922
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..