Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 1.48 g/micron | 37.5 g/mil | 2 mil; ASTM D1922 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |