Polymer Property : Elmendorf Tear Strength, TD = 389 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 15.3 g/micron
389 g/mil
ISO 6383-2
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film
This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be..