Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.25 g/micron | 108 g/mil | 50 µm (2 mil) film; ASTM D1922 |
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |
|||
Elmendorf Tear Strength, TD | 4.25 g/micron | 108 g/mil | Calculated from mfr's report of 10.8 N per TAPPI-414 and the typical thickness |
DuPont™ Nomex® 410 Paper, 10 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Elmendorf Tear Strength, TD | 4.25 g/micron | 108 g/mil | 50 µm (2 mil) film; ASTM D1922 |
DuPont Elvax® 3173SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
(discontinued **)< 18 wt% Vinyl Acetate.Elvax® 3173SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res.. |