Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM D1922 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ISO 6383-2 |
Total EVA 1020 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 5 is made by a high pressure tubular process. Grade for very flexible films with very high transparency and good mechanical properties. Contains an antioxidant.Application examples: Ch.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM D1922 |
Braskem BF 2021 LDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Films for absorbents and diapers (with HDPE and LLDPE); general purpose. Information provi.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM-D1922 |
Braskem F2523 LDPE Blown Film Extrusion Polyethylene LDPE F2523 is a low-density polyethylene. It has good sealing characteristics, optical, and mechanical properties. It contains antiblock and slip additives. Its applications include general purpose .. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM-D1922 |
Braskem TS7003 LDPE Blown Film Extrusion Polyethylene TS7003 is a low-density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed. Th.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM D1922 |
Braskem EB 861/51 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Coextruded films; Shrink films for pallets; general purpose. Information provided by Brask.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM D1922 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |
|||
Elmendorf Tear Strength, TD | 4.40 g/micron | 112 g/mil | ASTM-D1922 |
Braskem TX7003 LDPE Blown Film Extrusion Polyethylene TX7003 is a low-density, high molecular-weight polyethylene that offers high mechanical strength. The product's characteristics allow for high versatility and use in various applications due to its .. |