Polymer Property : Elmendorf Tear Strength, TD = 480 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD >= 18.9 g/micron
>= 480 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 5117N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, TD >= 18.9 g/micron
>= 480 g/mil
ASTM D1922
NIZHNEKAMSKNEFTEKHIM PE 5118N (18601) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Elmendorf Tear Strength, TD 18.9 g/micron
480 g/mil
ASTM D1922
ExxonMobil Exceed™ 1023DA Tough Premium Film Resin  (discontinued **)
Exceed 1023DA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023DA resin have outstanding tensile, impact strength and puncture. These superi..
Elmendorf Tear Strength, TD 18.9 g/micron
480 g/mil
Westlake LF1021 Butene Linear Low Density Polyethylene
Westlake LF1021 is a butene LLDPE with excellent mechanical and downgauging advantages. It is suitable for can liners, stretch wrap, agricultural film, and blending with LDPE. This Kosher compliant ..