Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 20.18 g/micron | 512.5 g/mil | ASTM D1922 |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |