Polymer Property : Elmendorf Tear Strength, TD = 554 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 21.8 g/micron
554 g/mil
Dow ATTANE™ 4301 Ultra Low Density Polyethylene, Blown Film Grade
ATTANE® 4301 copolymer is an ultra low density polyethylene having high impact resistance and tear strength in blown films, designed for use in food packaging applications. It has low levels of sli..
Elmendorf Tear Strength, TD 21.8 g/micron
554 g/mil
Dow ATTANE™ 4701 Ultra Low Density Polyethylene, Medical Packaging Grade
ATTANE® 4701 copolymer is an ultra low density polyethylene having high pinhole and puncture resistance, tear strength and high impact resistance combined with improved softness. It has low levels ..