Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 23.0 g/micron
584 g/mil
ASTM D1922
Polymer Industries Densetec HDPE Rod
Polymer Industries’ HDPE Rod exhibits all the durable qualities found in Densetec HDPE Sheet, making it perfect for that industrial application where sheet stock is not suitable. The HDPE Rod is av..
Elmendorf Tear Strength, TD 23.0 g/micron
584 g/mil
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin
17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..
Elmendorf Tear Strength, TD 23.0 g/micron
584 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur..
Elmendorf Tear Strength, TD 23.0 g/micron
584 g/mil
ASTM D1922
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer.
Elmendorf Tear Strength, TD 23.0 g/micron
584 g/mil
ASTM 1922
Braskem Flexus® 7200 LLDPE Cast Film Extrusion
Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing..
Elmendorf Tear Strength, TD 23.0 g/micron
584 g/mil
ASTM D1922
NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent seal characteristics.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufacturer.