Polymer Property : Elmendorf Tear Strength, TD = 6.70 g/micron
Polymer Property :
Elmendorf Tear Strength, TD =
6.70 g/micron
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Elmendorf Tear Strength, TD
6.70
g/micron
170
g/mil
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.