Polymer Property : Elmendorf Tear Strength, TD = 6.7492 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 6.7492 g/micron
171.43 g/mil
propagated; ASTM D1922
Honeywell Capran® NyLid™ WMB 175 Nylon Lidding Film  (discontinued **)
Description: Capran® NyLid™ WMB 175 is a 1.75 mil, white medium barrier nylon co-extruded film with an EVOH core. Applications: Capran® NyLid™ WMB 175 is suitable for die cutting, readily accept..