Polymer Property : Elmendorf Tear Strength, TD = 6.99 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 0.275 g/micron
6.99 g/mil
ISO 6383/2
Borealis Borstar® FB2230 LLDPE for Film
Borstar BF2230 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from ..
Elmendorf Tear Strength, TD 0.275 - 135 g/micron
6.99 - 3430 g/mil
Average value: 21.8 g/micron Grade Count:175
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..