Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 2.63 g/micron
66.8 g/mil
ASTM-D1922
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene
PB681 is a resin produced under high pressure in a tubular reactor. This resin presents excellent 'draw down' (stability to form fine films). The films produced with this resin have excellent optica..