Elmendorf Tear Strength, TD 7.24 g/micron
184 g/mil
ASTM D1922
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow