Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 30.8 g/micron | 782 g/mil | ASTM-D1922 |
Braskem LL5800N LLDPE Blown Film Extrusion Polyethylene Copolymer LL5800N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing aid .. |
|||
Elmendorf Tear Strength, TD | 30.8 g/micron | 782 g/mil | ASTM-D1922 |
Braskem LL5801N LLDPE Blown Film Extrusion Polyethylene Copolymer The LL5801N resin is a linear low-density polyethylene, copolymer of octene-1, produced by the solution process for blown film extrusion with excellent mechanical properties. It contains processing .. |