Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 31.939 g/micron
811.25 g/mil
ASTM D1922
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7066 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. Th..