Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 9.83 g/micron | 250 g/mil | ASTM D1922 |
SCG Chemicals EL-Leneâ„¢ H5615F High Density Polyethylene Film Key Characteristics:High speed processingHigh tensile strengthHigh dart impactLow gel contentGood moisture barrierRecommended Applications: Ultra thin film ( |