Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Elmendorf Tear Strength, TD = 93.33 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 3.674 g/micron
93.33 g/mil
ASTM D1922
ExxonMobil LD 313.NF Blown Film Resin
LD 313.NF is a 3 wt% vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopolymers.Information pr..
Copyright © lookpolymers.com All Rights Reserved