Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 89.0 g | 0.196 lb | Method A; ASTM D1709 |
Dow 650I Low Density Polyethylene Resin DOW LDPE 650I Resin is intended for use in soft goods over wrap, bread bags, shrink films and other general purpose applications.Information provided by Dow |