Mechanical Properties Metric English Comments
Dart Drop Test 370 g
0.816 lb
F-50 at 26 in.; ASTM D1709
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Dart Drop Test 370 g
0.816 lb
D1709
Westlake EF524 14.5% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF524 is an ethylene vinyl acetate copolymer with 14.5% VA. EF524 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength..
Dart Drop Test 370 g
0.816 lb
ASTM D1709A
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate
Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast..
Dart Drop Test 370 g
0.816 lb
ASTM D1709A
ExxonMobil Escorene® LD 720.01 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Dart Drop Test 370 g
0.816 lb
ASTM D1709A
ExxonMobil Escorene® LD 720.62 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Dart Drop Test 370 g
0.816 lb
ASTM D1709
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade
Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i..
Copyright © lookpolymers.com All Rights Reserved