Mechanical Properties Metric English Comments
Dart Drop Test 440 g
0.970 lb
F-50 at 26 in.; ASTM D1709
Chevron Phillips Vytek™ V208C6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Dart Drop Test 440 g
0.970 lb
ASTM D1709
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell..