Dart Drop Test 900 g
1.98 lb
ASTM D1709
ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes..
Dart Drop Test 900 g
1.98 lb
ASTM D1709
ExxonMobil Exceed™ 1012HJ Metallocene Polyethylene Resin
Product Description: Exceed 1012 mVLDPE resins are metallocene ethylene-hexene copolymer. Films made from these resins have outstanding cold temperature toughness, impact strength and puncture. Thes..