Polymer Property : Dart Drop Test = 105 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 105 g
0.232 lb
ASTM D1709
SABIC 118 Series Linear Low Density Polyethylene for Blown Film
Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st..
Dart Drop Test 105 g
0.232 lb
F50; ISO 7765-1
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit..
Dart Drop Test 105 g
0.232 lb
F50; ISO 7765-1
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe..
Dart Drop Test 105 g
0.232 lb
F50; ASTM D-1709
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su..
Dart Drop Test 105 g
0.232 lb
ASTM D1709A
LyondellBasell Montell 16501F3 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA..
Dart Drop Test 105 g
0.232 lb
ASTM D1709A
LyondellBasell Montell 16501F4 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets F..
Dart Drop Test 105 g
0.232 lb
ASTM D1709A
LyondellBasell Montell 16501F6 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMeets ..
Dart Drop Test 105 g
0.232 lb
ASTM D1709A
LyondellBasell Montell 16501F7 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet..
Dart Drop Test 105 g
0.232 lb
ASTM D1709A
LyondellBasell Montell 16501F8 Butene LLDPE
Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee..
Dart Drop Test 105 g
0.232 lb
JPJ Technologies LLD150-2 LLDPE Virgin
Application: Used for ice & frozen bags, garbage bags consumer packingInformation provided by JPJ Technologies
Dart Drop Test 105 g
0.232 lb
F50; ASTM D1709 A
Equate EFDA-7047 LLDPE Film Extrusion Resin
EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n..
Dart Drop Test 105 g
0.232 lb
F50; ASTM D1709 A
Equate EFDC-7087 LLDPE Film Extrusion Resin
EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-..