Dart Drop Test 30.0 - 1350 g
0.0662 - 2.98 lb
Average value: 250 g Grade Count:164
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..