Mechanical Properties Metric English Comments
Dart Drop Test 148 g
0.326 lb
Method B; ASTM D1709
Dow DOWLEX™ 2247G Polyethylene Resin
Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap..