Mechanical Properties Metric English Comments
Dart Drop Test 165 g
0.364 lb
(method A); ASTM D1709
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film..
Dart Drop Test 165 g
0.364 lb
ASTM D1709
Huntsman PE1407 EVA Film Extrusion  (discontinued **)
4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..