Mechanical Properties Metric English Comments
Dart Drop Test >= 1000 g
>= 2.20 lb
ASTM D1709/A
NOVA Chemicals Sclair® FP112-A Octene VLDPE Film Resin
Features: Low seal initiation temperatureHigh toughnessVery good optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Low gel Applications: Sealant and lamination film for food packagi..
Dart Drop Test >= 1000 g
>= 2.20 lb
F50; ASTM D1709
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng..
Dart Drop Test >= 1000 g
>= 2.20 lb
50µ; ISO 7765-1
Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding  (discontinued **)
EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f..
Dart Drop Test >= 1000 g
>= 2.20 lb
50µ; ISO 7765-1
Total Evatane® 28 - 03 HDPE, blown film  (discontinued **)
EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f..
Dart Drop Test >= 1000 g
>= 2.20 lb
50µ; ISO 7765-1
Total Evatane® 28 - 05 HDPE vinyl acetate copolymer, blown film, injection molding  (discontinued **)
EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 120 to 150.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f..
Dart Drop Test >= 1000 g
>= 2.20 lb
Using 2 in. (0.508 cm) dia dart, 60 in. (774 cm) drop height.
Kraton® D1102 + LDPE blend (50/50)
Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A..
Dart Drop Test >= 1000 g
>= 2.20 lb
Method B; ASTM D1709
Styrolution Styroflex® 2G 66 SBC
Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o..
Dart Drop Test >= 1000 g
>= 2.20 lb
ASTM D1709
M. Holland Company MAGMA® LM311-DX LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Dart Drop Test >= 1000 g
>= 2.20 lb
ASTM D1709
M. Holland Company MAGMA® LM311-D LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.