Polymer Property : Dart Drop Test = 2.43 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test >= 1100 g
>= 2.43 lb
26 in; ASTM D1709
Chevron Phillips MarFlex® D143 m-LLDPE Linear Low Density Polyethylene
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..