Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 30.0 - 300 g | 0.0662 - 0.662 lb | Average value: 124 g Grade Count:16 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |