Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 50.0 - 60.0 g | 0.110 - 0.132 lb | ASTM D1709 |
LyondellBasell Petrothene® M2520FN Low Density Polyethylene ApplicationsPETROTHENE M 2520 is a film grade resin that exhibits excellent optics, good gloss and good bubble stability. A typical application for this resin is high clarity packaging. Regulatory.. |