Mechanical Properties Metric English Comments
Dart Drop Test 400 - 600 g
0.882 - 1.32 lb
Average value: 550 g Grade Count:4
Overview of materials for Nylon 66, Film
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat..