Mechanical Properties Metric English Comments
Dart Drop Test 650 g
1.43 lb
26 in; ASTM D1709
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene  (discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..
Dart Drop Test 650 g
1.43 lb
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Dart Drop Test 650 g
1.43 lb
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Dart Drop Test 650 g
1.43 lb
ISO 7765-1
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: ..
Dart Drop Test 650 g
1.43 lb
ASTM D1709A
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 730.09 is a 17.2% vinyl acetate copolymer film resin. LD 730.09 is designed to have superior strength and toughness combined with excellent optics and sealing ..
Dart Drop Test 650 g
1.43 lb
F50; ISO 7765-A
Carmel Olefins IPETHENE® 4203 Low Density Polyethylene
IPETHENE® 4203 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, very good bubble stability in thick-gauge blown film processing, and excellent ESCR. ..
Dart Drop Test 650 g
1.43 lb
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Dart Drop Test 650 g
1.43 lb
F-50 at 26 in.; ASTM D1709
Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..