Mechanical Properties Metric English Comments
Dart Drop Test >= 800 g
>= 1.76 lb
ASTM D1709/A
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin
Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat..
Dart Drop Test 800 g
1.76 lb
ASTM D1709
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene
Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-..
Dart Drop Test 800 g
1.76 lb
ASTM D1709/A
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin  (discontinued **)
Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals