Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 6980 MPa @Pressure 30.0 MPa, Temperature 23.0 °C |
1.01e+6 psi @Pressure 4350 psi, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Creep Modulus, 1 hour | 6990 MPa @Pressure 20.0 MPa, Temperature 23.0 °C |
1.01e+6 psi @Pressure 2900 psi, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |