Polymer Property : Tensile Creep Modulus, 1 hour = 1.04e+6 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 7200 MPa

@Time 3600 sec
1.04e+6 psi

@Time 1.00 hour
ISO 899-1
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..