Tensile Creep Modulus, 1 hour 1020 MPa

@Pressure 8.00 MPa,
Temperature 23.0 °C
147000 psi

@Pressure 1160 psi,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers