Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 3570 MPa @Pressure 5.00 MPa, Temperature 100 °C |
518000 psi @Pressure 725 psi, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 3570 MPa @Pressure 10.0 MPa, Temperature 100 °C |
518000 psi @Pressure 1450 psi, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 3570 MPa @Pressure 15.0 MPa, Temperature 100 °C |
518000 psi @Pressure 2180 psi, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 3570 MPa @Pressure 20.0 MPa, Temperature 100 °C |
518000 psi @Pressure 2900 psi, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 3570 MPa @Pressure 25.0 MPa, Temperature 100 °C |
518000 psi @Pressure 3630 psi, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1 hour | 3570 MPa @Pressure 30.0 MPa, Temperature 100 °C |
518000 psi @Pressure 4350 psi, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |