Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1 hour 621 MPa

@Pressure 6.00 MPa,
Temperature 60.0 °C
90100 psi

@Pressure 870 psi,
Temperature 140 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers