Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 2380 MPa

@Pressure 5.00 MPa,
Temperature 23.0 °C
345000 psi

@Pressure 725 psi,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)