Polymer Property : Film Tensile Strength at Break, TD = 1050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 7.24 MPa
1050 psi
ASTM D882
LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (0.5 mil Film)
ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die b..