Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 80.0 MPa
11600 psi
ISO 527
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled
APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application..
Film Tensile Strength at Break, TD 80.0 MPa

@Thickness 0.0250 mm
11600 psi

@Thickness 0.000984 in
ISO 527
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled
APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application..
Film Tensile Strength at Break, TD 80.0 MPa

@Thickness 0.100 mm
11600 psi

@Thickness 0.00394 in
ISO 527
Victrex® APTIV® 1102-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 20% Mineral Filled
APTIV PEEK 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance application..
Film Tensile Strength at Break, TD 80.0 MPa
11600 psi
ASTM D882
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..