Polymer Property : Film Tensile Strength at Break, TD = 12.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 12.4 MPa
1800 psi
ASTM D882
Dow DAF 780 Carpet Underlayment Adhesion Film
DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow