Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 84.8 MPa | 12300 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Metallyte™ UHB 35 MWHB OPP Film Product Description: A multi-layer, cavitaed, white OPP film structure that has exceptional barrier to gases and flavors. It is metalized on one side and treated on the other. It is designed for use.. |
|||
Film Tensile Strength at Break, TD | 85.0 MPa | 12300 psi | ISO 527-3 |
EMS-Grivory Grivory® G 25 PA6I/6T Product description: Grivory G 25 is a very high viscous amorphous copolyamide. It is suitable for injection stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of .. |
|||
Film Tensile Strength at Break, TD | 85.0 MPa | 12300 psi | ISO 527-3 |
EMS-Grivory Grivory® G 21 PA6I/6T Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle.. |