Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 13.5 MPa | 1960 psi | ASTM D882 |
ExxonMobil LD 145.PX Packaging Resin
(discontinued **) LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 13.5 MPa | 1960 psi | ASTM D3759 |
3M Scotch® 3199 Security Message Box Sealing Tape Scotch® Security Message Box Sealing Tape 3199 is a performance packaging tape used specifically where the security of the carton contents is a concern. The printed design along with the message ma.. |