Polymer Property : Film Tensile Strength at Break, TD = 135 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 135 MPa
19600 psi
ASTM D3759
3M Scotch® 311 Box Sealing Tape
Scotch® Box Sealing Tape 311 is a general purpose box sealing tape designed specifically for utility type applications on light to medium weight boxes. The product offers good performance over broa..