Polymer Property : Film Tensile Strength at Break, TD = 14500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 53.8 - 100 MPa
7800 - 14500 psi
ASTM D882
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film
Description: Oxyshieldâ„¢ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro..
Film Tensile Strength at Break, TD 60.0 - 100 MPa
8700 - 14500 psi
Average value: 80.0 MPa Grade Count:5
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..