Polymer Property : Film Tensile Strength at Break, TD = 1740 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD >= 12.0 MPa
>= 1740 psi
ASTM D882
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE  (discontinued **)
Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell..
Film Tensile Strength at Break, TD 12.0 MPa
1740 psi
ASTM D882
ExxonMobil Escorene® LD-734 High EVA Extrusion Coating Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and..